Coating Tech Slot Dies

Coating Tech Slot Dies

By Coating Tech Slot DiesNewsTech News
Download on the App Store

All Coating Tech Slot Dies episodes

  • Lane Coating with Slot Die Equipment
    /wp-content/uploads/Lane-Coating-with-Slot-Die-Equipment.mp3
    DOWNLOAD AUDIO FILE

    Whether coating batteries or adhesive tapes, there are reasons why coating full width is not always optimal.  When an operation lends itself to coating wet and dry lanes down web across a substrate, what is required to understand what is involved?

    Lane coating is the process of taking a fully formed precision flow of fluid and breaking it into areas of coated and uncoated areas as the substrate moves down web.  This appears as lanes of coated fluid with dry lanes in between.  This patterned coating can be achieved with any coating technique by placing barriers to the flow path.  In slot die coating, this means that the flow area needs to be controlled both inside and outside the flow cavity of the coating head.

    Inside the slot die, the flow control can simply be the placement of a seal at the exit point of the slot die.  In a fixed lip style slot die, where the slot gap is held open by a body shim, the body shim would simply need to be manufactured with “fingers” that run from the manifold back line to the exit point of the slot die where the fluid would be kept from exiting.  The open spaces between the fingers would allow for fluid flow and the full manifold would still be employed to distribute the flow correctly.  In a flexible lip style slot die, where the slot gap is controlled by adjustable screws, a metal or plastic deckle would be placed in the front face of the slot die between the upper and lower lip and the adjusting bolt would be clamped down on the deckle.  Care needs to be taken with an adjustable lip slot die to make sure that the spacing of the adjusting lip and the deckle size correlate.  Adjustable lip bolts should work in groups of 3 across the solid lip assembly and spacing of the adjustable screws are typically 1 inch (25.4 mm) or more.  If a narrower spacing is required, an external shim may need to be considered.

    The lane dimensions are limited to the internal flow, the external flow and the physical geometry of the shim being developed.  Once the shim geometry becomes narrow, a serrated lip may need to be considered.  A serrated lip would have the coated and uncoated areas cut and ground into the lip land itself.  This permanent feature should only be considered after the experimentation is complete to understand how the fluid reacts with the substrate at operating conditions of production.

    When the fluid to be coated is reduced from full width to something less, the manifold is running sub-optimally.  With this sub-optimal flow, internal flow analysis will make sure that turbulence and residence time doesn’t become an issue, but experimentation will still be required to understand what is going on outside the coating head.  A rule of thumb is to have the manifold run optimally requires that full width coating takes place down to 20% less than full width coating.  In lane coating, these uncoated sections can add up and produce flow areas that reduce the flow control of the slot die manifold cavity design.

    Computer modeling reduces guess work and provides precise understanding of the internal flow control, but the boundary conditions and mathematical analysis of external flow is limited.  The liquid can be understood according to the Navier-Stokes equation, but surface energy and surface tension interaction along with wetting and spreading phenomenon are not described by the math involved.  Because of this lack of capability to simulate flow outside the slot die, experiments should be run within the production process conditions to understand how the fluid will react to the substrate after exiting the slot die.  This may lead to shim dimension variations and iterative design and manufacturing of flow control features.

    The ultimate goal is to reduce converting steps and not have wasted fluid coated onto the substrate of choice.  With simulation support and experimental guidance, lane coating and efficient coating can be developed.

    14 min
  • The Importance of the Positioner in Slot Die Coating
    /wp-content/uploads/The-Importance-of-the-Positioner-in-Slot-Die-Coating-.mp3
    DOWNLOAD AUDIO FILE

    INTRODUCTION

    The slot die coating positioner.  That’s not even a real word!  If you type in the word positioner, the word processing program complains that you didn’t spell positioned correctly.  Well, the software developers didn’t work in the coating and converting industry.  For those of us who do, the positioner, or mounting equipment for the slot die is critical to fluid coating application.

    In standard proximity coating, a slot die is held the wet coating distance away from the substrate, which is supported by a precision backing roll.  But what is holding the slot die in place?  The mounting system that holds the slot die within microns of the proper coating position is referred to as a positioner in coating manufacturing circles.  As products are coated thinner and more precisely, the potential variation in the slot die to substrate gap can be the difference in precision coated products and scrap.

    The positioner has some key features that make it work properly.  Mechanically, the slot die mounting system should be designed to not twist or torque under the movement and pressures associated with the slot die interaction.  Finite element analysis of the mechanical structure is recommended during the design phase.  Movement along linear bearings allow for precision control and smooth transition from the off-coat to the on-coat position.  Pneumatic actuation is common, but servo motors can allow for improved repeatability and less settling time, although the strength of the motor versus the back pressure in the slot die to roll operation should be considered.

    Setting the gap initially is important to flow control at the exit of the slot die, but repeatability is also important.  If the substrate requires a splice to pass, the positioner is the equipment that jumps the splice with a micro movement.  Having the positioner return to the coating position quickly and repeatably allows the coating to continue with very little interruption.  If the coating line needs to stop for an extended period of time, the positioner allows the slot die to be retracted a distance that allows the operator to clean the front face with no potential of interfering with the substrate or precision roll.  This coarse adjustment is typically 6 inches (152 mm) or more.  The splice jump movement is enough to allow the splice to pass without keeping the slot die disengaged too long.  Repeatability is typically 0.0001 inch (2.54 microns).

    A positioner is not only critical in proximity coating.  In tensioned web over slot die (TWOSD) coating technique, a uniform placement of the slot die in relation to the web tensioned over the slot die is paramount.  Skew in the slot die to substrate position could lead to cross web coating non-uniformity, wrinkling or coating defects.

    In hot melt adhesive coating, the positioner has the added function of controlling the attack angle of the slot die to the backing roll.  Because of the stronger elastic characteristic of hot melt adhesives, the variation of the attack angle plays an important role for successful coating.  The rotation of the slot die should be around the lower corner of the upper lip (coating in a horizontal position).  Rotating in another location of the slot die will lead to improper geometric changes and having to shift the die to coat correctly.

    There are 2 critical gaps in slot die coating technology, the slot die opening itself and the gap between the slot die and the substrate.  While the slot die opening is more critical and controlling a cubic volumetric flow value, the positioner controls the linear relationship of flow control at the exit point of the slot die.  If the coating bead at the dynamic wetting line is not stable, neither will the flow control.

    The positioner controls the coating bead development which keeps out air and develops the meniscus across the length of the slot die lip face.  The variations in pressure from the upstream to the downstream portion of the fluid flow can be successfully managed through this gap control and proper lip offset.  In the common coating defects seen in fluid applications to substrates, some of the most common are related to the slot die to substrate gap which the positioner controls.

    Position your slot die properly and enjoy coating success!  Regardless of whether a positioner is a real word or not.

    14 min
  • Curtain Coating Technology
    /wp-content/uploads/CURTAIN-COATING-TECHNOLOGY.mp3
    DOWNLOAD AUDIO FILE

    INTRODUCTION

    Economies of scale occur when a coated product is manufactured wide, fast and in one pass. Substrates can be manufactured wide and multilayer coating can provided added functionality, but how do you make a coated product faster. The first hurdle is curing (typically the bottleneck of the process). Once you properly size the oven for the application, you need to consider the fluid flow dynamics within the coating system. As the fluid is coated faster and faster, the effects of film split, turbulence and air reek havoc on the coated product and leave a trail of coating defects in the path.

    Some coating techniques, however, actually perform better under high speed scenarios. One coating technique that should be considered for high speed applications is curtain coating. Imagine taking a slot die, coating in close proximity, and raising it up in the air to allow the fluid to drop down onto the substrate. This rain shower of liquid can have some advantages, but the advantages can only be realized with higher speeds. Why is that?

    The fundamental equation behind the success of a falling curtain of fluid is the dimensionless Weber number-

    We = ρQV/σ 

    We = Weber number

    ρ = density 

    Q = volumetric flow rate 

    V = impingement velocity 

    σ = surface tension 

    The Weber number provides us with the height of the curtain that allows for success. A good starting point is to look for the coating conditions that allow for We > 2. This is considered a stability region for the fluid. As We < 2, the constant flow of fluid breaks up and disintegrates into droplets instead of a sheet. While it is possible to maintain a curtain under many conditions, this gets us started. Let’s break it down. The Weber number is a ratio of the density, volumetric flow rate and fluid flow rate to surface tension forces. The fluid flow rate is also termed the impingement speed of the fluid – the higher the fluid falls the faster the speed. Line speed and pump work together to develop the coat weight of the product – for a set pump speed (volumetric flow rate), a higher line speed creates a lighter coat weight product. Now, if the fluid is dropped at a high throughput, but the line speed is slow, the coat weight will be high. So if your product requires a light coat weight, you will need to adjust height or flow rate to meet our stability criteria (We > 2). Since density and surface tension are relatively set, volumetric flow rate or height of the curtain are the only variables that can be shifted to land the product in a reasonable coating window.

    Now, there are many variables that affect the flow and stability of curtain coating a fluid, but the Weber number stability criteria is a good starting point. The coating window itself is a function of the Reynolds number and the web speed to impingement velocity-

    Re = ρQ/μ 

    Re = Reynolds number 

    ρ = density 

    Q = volumetric flow rate 

    μ = viscosity 

    U/V 

    U = web speed 

    V = impingement velocity 

    If the U/V ratio is too low, disintegration of the curtain occurs (similar to a low Weber number). At a balance point between Re and U/V, the coating is stable. As U/V increases, we begin to see air be an issue because the line speed overcomes the fluid velocity.

    With this handful of variables and simple equations, you can evaluate curtain coating to improve your speed and move into a new realm of coating capability.

    ADVANTAGES

    At its basic level, curtain coating differs from proximity coating only the distance from the substrate.  Besides this distance, many of the basic physical characteristics apply.  Both systems develop a meniscus, dynamic wetting line and free surface.  Both require precision machined edges and faces of the slot die to perform well.  Both techniques can coat as multi-layer systems to produce coated systems with multiple functional layers.  Also, both proximity coating and curtain coating technique need proper development of the fluid substrate interface to reduce air entrainment.

    For proximity coating, a slot die is positioned the wet coating thickness away from the substrate.  For curtain coating, the gap is much larger and determined not only by the wet coating thickness, but the web speed, impingement velocity, density and viscosity of the fluid being coated.  This extra distance allows for coating irregular surfaces that would not normally be proximity coated.  Examples include nonwoven substrates and glass panels.

    Hydrodynamic assist is a function of distance from the slot die exit to the substrate, gravitational orientation compared to direction of fluid flow, and momentum of the fluid at the impact with the substrate.

    Whether coating a continuous sheet or a discrete part, curtain coating provides a speed advantage that may be a limitation for proximity coating.  In the early years of curtain coating, the liquid was released in a fluid film over parts and pieces and any excess liquid was collected and recirculated for continuous use.  This is still an option, but if solvents are released during operation, a recovery system should measure the density and viscosity to replace the proper amount of solvent during the recovery process.

    So how fast do you need to run the line, how high does the slot die need to be from the substrate and how much fluid needs to be pumped through the slot die to form a stable curtain?  Every fluid and substrate interaction is different because of rheology and interfacial dynamics, but a good rule of thumb is that the flow rate of 0.5 cm3/s at a height of 250 mm (9.84 inches) works well for most applications.

    Similar to proximity coating with slot die technology, finite element analysis can be completed to verify that the internal flow is appropriate for a stable cross-web caliper liquid curtain.  This information can verify that the liquid curtain will be robust enough to develop flow that has the same velocity, same pressure drop and same volumetric flow at exit.

    DISADVANTAGES

    The lengthy fluid bridge that is created in a curtain coating technique is fundamentally different than the short fluid  bridge created in proximity coating with slot die technology.  Instead of needing to cover the wet coating thickness through the formation of a meniscus at the substrate and slot die interface, curtains that are formed need to be self-supported until they reach the point of substrate interaction where the hydrodynamic assist develops the meniscus as required in all coating systems.

    This lengthy curtain of fluid can be disrupted by air flow or vibrations.  To have the best possible flow control a couple items are required:  sharp lips at the slot die exit to control the static contact line of the fluid; edge guides to control curvature of the fluid during flow from the slot die exit to the substrate; and air shields to control the environmental impact of air currents on fluid flow.

    To maintain a stable film formed to the complete width of the slot die coating exit, edge guides are required.  These can take the form of simple plates that the fluid rides from the slot die exit to the substrate or as complex as liquid fed tubes that help carry the curtain down.  The key is curtain stability at the edges.  Without mechanical edge guides, the liquid would neck in and have curvature in three dimensions.  This is most troublesome at the edges of the liquid formation, causing the fluid to curl in on itself and form edge beads that would be thicker than the rest of the coated substrate.

    Air shields protect the formed curtain from disruption during operation.  A simple air current developed from an air duct or door movement can break up a stable curtain.  These mechanical air shields need to be concerned with the fluid formation zones at the slot die exit, the curtain stability zone during the travel from the slot die exit to the substrate and the coated film formation zone at the substrate.

    In addition to the air and vibration issues associated with an unsupported fluid curtain, the hydrodynamic assist function creates an operating limitation and a reduced coating window.  The way the fluid develops a heel at the point of impact is important.  This heel development is a function of the contact angle which is subsequently dependent on the line speed and the wettability of the fluid onto the substrate.  This wettability can be encouraged through surface energy and surface tension match making between the liquid and the substrate, but is more powerfully controlled by the substrate speed and the volumetric liquid flow.

    This ratio of volumetric flow (V) and substrate speed (U) is presented at the Reynolds number calculation. The ratio of U/V has a dramatic effect on the heel development of the impinged fluid flow.  While heel development needs to meet a critical level of stability for the removal of air, too large of a heel (too low of a substrate speed for the fluid flow) can lead to turbulent flow in the impinged heel and air defects downstream.  The exact Reynolds number and U/V ratio is empirically determined.

    The Weber number calculation provides a great starting point to understand where the fluid will form a stable curtain, but this needs to be combined with the understanding of the hydrodynamic assist concept to produce a usable coated product.  Past experience has shown that while the literature states that a Weber number greater than 2 should produce a stable curtain, a Weber number greater than 7 typically is required for a robust stable curtain.  This theoretical versus reality based idea should be considered when designing equipment and coating liens with little empirical data.

    Understanding the distribution of the liquid flow at the slot die exit is important for both proximity and curtain slot die coating operation.  This can be completed through finite element analysis and verified through experimentation.  However, developing a computer model of the flow external to the slot die in either arrangement is less simple.  The boundary conditions are less controlled which leads to a reduced understanding and replication with empirical data.  Navier-Stokes calculations provide a good starting point for a physics based concept of flow.  To further develop mathematical models, understanding the liquid to substrate interface should be empirically measured and compared to the FEA models being developed.

    In the observation of the heel formation in curtain coating projects, the hydrodynamic assist can lead to a stable meniscus and coated film or not.  The worst case scenario looks like a pulled film without any heel formation while an intermediary flow looks like a heel is formed, but disrupted and unstable.  In either case the issue is air entrainment.  Air entrainment will lead to uneven flow and potential streaks developing in the coated surface.  The volumetric flow needs to be increased or the substrate speed needs to be reduced.  Keeping in mind that the ratio of the two develops the proper coat weight for the product.

    CONCLUSION

    Curtain coating slot die technology is an ideal solution for coating irregular surfaces at high speed.  It should be considered an option whenever proximity coating is not an option or thinner coatings and higher line speeds are required to meet the economics of the coated product.  With every equipment setup, however, considerations need to be reviewed.  Balancing the advantages of increased coating gap, higher line speeds and thinner coatings, with the disadvantages of air disturbances, vibration disruptions and the minimum line speed and flow rate requirements, leads to a process equipment decision based on economics and capability.  Curtain coating provides a strong case for precision coating from a distance.

    REFERENCES

    1. A Mohammad Karim, WJ Suszynski, S Pujari, Liquid film stability and contact line dynamics of emulsion liquid films in curtain coating process. Journal of Coatings, V18, pp. 1531-1541 (2021)
    2. Chen-Yu Liu, Eric Vandre, Marcio S. Carvalho, Satish Kumar, Dynamic wetting failure and hydrodynamic assist in curtain coating. Journal of Fluid, V808, pp. 290-315 (2016) – cambridge.org
    3. 14 min
    4. Rigid Panel Coating with Slot Die Equipment

      /wp-content/uploads/Rigid-Panel-Coating-with-Slot-Die-Equipment.mp3
      Download Audio File

      INTRODUCTION

      Panel coating is a unique application of fluid coating technology that provides capability and functionality to a discrete substrate. But what is important to understand and what tradeoffs exist?

      Unlike continuous coating application against a moving substrate, we are trying to develop steady state control over an intermittent process. The fluid needs to exit the slot die only when we want it to and stop flowing before a mess is made. In intermittent coating there are a number of variables to consider.

      Like continuous coating, the math and physics involved to control flow and predict behavior for two dimensional laminar flow is the same. The trick is to develop quality coating immediately and stop the flow perfectly. So this head and tail development is more critical in rigid panel coating than it is in continuous coating.

      FLUID RHEOLOGY

      Many fluids can be coated onto rigid panels, so what are the key factors to be aware of in the fluid chemistry, surface energy and rheology to predict quality performance? One key factor is viscoelasticity of the fluid to be coated. In addition to the viscosity, elasticity can cause die swell, edge bead or ribbing. The external effects of fluid flow and viscoelasticity typically require some trial and error because predicting flow outside the slot die has fewer boundary conditions for simulation. Owning or having access to research and development level panel coaters are very helpful with new fluids or substrates.

      There are two main techniques for coating rigid panels – proximity and curtain coating. Both utilize slot dies, but each has a different set of criteria to develop successful performance.

      In proximity coating, the gap maintained between the slot die lip face and the rigid panel is 1-2 times the wet coating thickness. So, the lower the wet coat weight, the closer the slot die gets to the substrate. For rigid panels that have variation in surface caliper, this small gap can lead to variation in coating or damage to the substrate.

      For very light coat weights (less than 1 mil or 25.4 microns), curtain coating should be considered. For curtain coating, the critical calculation of success is the Weber number. No heavy math is required, just a simple understanding of the fluid and the equipment setup.

      We = ρQV/σ

      We = Weber number

      ρ = density

      Q = volumetric flow rate

      V = impingement velocity

      σ = surface tension

      This simple equation helps us determine the success of coating based off a couple of easy to find numbers from the fluid and process. Success is typically predicted when the Weber number is greater than 2. One thing that you will notice with this equation is that the volumetric flow rate needs to be high and therefore the line speed needs to be high for low coat weights. This may limit the equipment capability if the coat weight is low because of the acceleration required to enter the coating curtain.

      One of the big differences between proximity and curtain coating is the area coated. In proximity coating there is typically a dry border left on the substrate. With curtain coating, there will be overcoat that needs to be dealt with.

      EQUIPMENT DESIGN

      How about the equipment utilized? First of all, the slot die is going to be positioned vertically. Why does this matter? Air. Evil air. When the fluid initially fills the manifold of the slot die, the air in the system wants to rise to the highest point. For a vertically oriented slot die, this means that the air will travel to the back of the manifold or the joint of attachment for the fluid delivery pipe or tube. If the air has no release mechanism, then the air will slowly release over time, causing coating defects. Ideally, a purge valve will be placed either in the back line of the manifold or the fluid delivery tube, whatever the highest point in the system is. Once the slot die is filled and purged, the air will release and then operate correctly. Without a purge mechanism, intermittent coating will fail forever, due to pressure variations.

      Intermittent coating is also subject to start and stop phenomenon. To relieve the pressure jolts that would occur with a valve with back pressure releasing a fluid into the slot die manifold and creating a heavy starting edge bead, a recirculation loop should be provided back to the day tank. Maintaining pressure within the entire circuit is critical to performance. The head and tail coated on the panel are a function of the stability of the pressure in the fluid delivery system in combination with the valve control and mechanical movement of the equipment.

      OPERATION

      After the equipment is set-up correctly, the coating of the rigid panel can still have issues. These issues can include the variation in the substrate, control of the travel and potential environmental factors. Let’s break these down a little.

      Especially in glass substrates, the surface flatness can vary tremendously. If the final product requires micron level control, and the equipment is precisely manufactured to deliver micron level performance, the product may still fail if the substrate variation exceeds the coating specification. Make sure that the substrate flatness meets or exceeds the flatness requirement for coating caliper control both cross web and down web.

      Another key factor in the coating of rigid panels is how to properly handle the substrate. Should the slot die move over the panel or should the panel move under the slot die? Can the panel be held stable with a vacuum table, or will the suction cause damage to the substrate? These factors need to be considered to properly design the equipment. Consider the stability and weight of the equipment traveling during the process. Also consider the ability to maintain precision as a heavy and stable piece of equipment traverses the coating area.

      Environmental factors come into play for both proximity and curtain coating, but more so in curtain coating. Because of the larger gap created in curtain coating we have to be concerned with air in the room disrupting the curtain. With proximity coating, room air won’t cause a fluid disturbance to the same extent as curtain coating, but mechanical vibration and environmental debris can cause coating defects. Make sure the fluid and substrate are clean before coating.

      CONCLUSION

      Rigid panel coating is becoming more and more common place. Understanding the variables to consider will help your company attack this multi-variable process with the right tools for success. If you work through the questions presented here, you will have a deeper understanding of how to successfully coat panels and limit coating defects.

      8 min
    5. Advances in Slot Die Coating Technology for Hot Melt Adhesives

      /wp-content/uploads/Advances-in-Slot-Die-Coating-Technology-for-Hot-Melt-Adhesives.mp3
      Download Audio File

      INTRODUCTION

      When it comes to fluid coating onto substrates, the equipment required falls into three areas-

      • Extrusion coating
      • Hot melt coating
      • Liquid coating
      • What makes these three coating methods the same and what makes them different?

        Extrusion coating is typically non-tacky molten polymers being cast onto substrates with a nipped roll and a large air gap. In extrusion coating, the coating head is directly fed from an extruder. Hot melt coating is typically tackified polymer adhesives that behave similar to molten polymers, but engage with the substrate in a proximity arrangement. Hot melt coating heads are fed by a precision metering pump being fed by an adhesive melter. Liquid coating resembles the proximity arrangement of hot melt coating, but the fluid is flowing at room temperature. Unlike extrusion and hot melt coating, liquid coating requires some form of curing to solidify the liquid on the substrate. Extrusion coating utilizes cooling to develop a solid film coating, while hot melt adhesive coatings solidify from cooling or curing.

        In pre-metered coating of extrusion, hot melt and liquid coating, the slot die design is very similar. If the rheological characteristics of the polymer, adhesive or liquid is identical, then the internal manifold cavity of the slot die would be identical also. So why does an extrusion coating head, a hot melt coating head and a liquid coating head look so different.

        An extrusion coating head has adjustable internal deckle flags that allow the operator to tune the polymer melt curtain flowing out of the slot die over the large gap between the slot die exit and the roll nip. Without this tuning capability, the extruded polymer melt curtain would neck in and have heavy edge beads. This tuning deckle reduces, but does not eliminate, these edge beads. Because polymer melts need to exit the slot die and not hang up on the lip faces, sharp edges to the lip face geometry is helpful.

        A hot melt slot die operates without the gap and nip arrangement of extrusion coating. This proximity coating arrangement, where the slot die lip faces are 1-2 times the coating thickness from the substrate, allow the slot die to operate without forming the edge bead and neck-in associated with extrusion coating. However, with the narrow gaps associated with proximity coating, different lip geometries may be needed for different coating thicknesses.

        Liquid coating slot dies are operated at room temperature. So while the external design of the slot die is very different from a hot melt and extrusion coating die, the internal functionality is very similar. As the fluid enters the slot die, it is controlled by the manifold cavity to exit the slot die at the same pressure, velocity and volumetric flow rate across the entire opening. Because temperature does not influence the slot die operation, the equipment can be manufactured and maintained to set gaps and tolerances. So for an ambient temperature application a fixed design for the slot die bodies and utilizing a shim creates the best operating condition.

        What happens if you add heat to the fluid? At some point, the metal starts to move. With the slot die body moving, an operator needs the ability to adjust the slot die back to the precise position that is required for precision coating operation. That is why the hot melt slot die and extrusion coating die are designed with a flexible lip design. Utilizing a flexible lip design for an ambient temperature coating adds variability that will make coating less precise. However, in a heated application, the lack of adjustability will not allow the slot die to provide the precision required.

        So, for hot melt adhesive coating, you need to understand the proximity coating arrangement of liquid coating while adjusting the slot die similar to an extrusion coating application. With this added complication, why would a company opt for hot melt coating over liquid coating? Well, while hot melt coating requires additional process knowledge to operate effectively, liquid coating requires additional curing that can create a rate limiting step in the process. If the liquid is solvent based, there is the additional environmental concern and cost. In order to understand the details of implementing hot melt coating, more background is required.

        ADHESIVE RHEOLOGY (VISCOSITY AND ELASTICITY)

        In hot melt adhesive coating, we are fundamentally coating rubber bands. Unlike many liquid coatings, hot melt adhesives have both viscous and elastic characteristics. This means that the adhesive polymer melt doesn’t just change the viscous flow characteristics with shear, but the adhesive may snap back after being stressed. This added effect can create unique coating defects not seen in liquid coating.

        The adhesive may act one way when being stressed and another upon relaxation. This difference, or hysteresis, of the polymer melt can create die swell, edge beads or film split upon coating. The more rheological knowledge you can have regarding the adhesive the better. And I’m not just talking about simple, single data point viscosity. A complex polymer melt requires a more sophisticated study of the flow effects. Develop testing protocols for complex rheology that show viscous and elastic behavior of the polymer under stress and shear will help an operator understand the variation in coating that may occur as lot-to-lot variation of the adhesive is presented to the coating head. Remember, the adhesive takes a tortuous path to the substrate. We need to understand the effects of the stress and design for both the viscous and elastic nature of the polymer for both the equipment and the process settings required for an economically viable coated product.

        Hot melt adhesives cover a wide range of applications, but the fundamental chemistries associated with EVAs, PURs and PSAs are all based off tackified polymers applied to substrates at elevated temperatures. Hot melt adhesives provide a functional character to the substrate for temporary or permanent bonding to a future surface after converting. These adhesives can be purchased or compounded in-house. These on-site compounds should be done with a word of caution. A slot die requires a consistent feed of adhesive with minimal lot-to-lot variability. If the adhesive and feed system is not consistent, the coating operator will chase the variation for the entire time the coating system is in operation. Until the volumetric flow and pressure of the adhesive delivery system is stable and the lot-to-lot adhesive chemistry is stable, the coating will vary.

        In complex rheological studies, we gain an understanding of whether the viscous or elastic characteristics dominate. If there is a time dependence on the loss or storage modulus in the complex rheological study, then elasticity overpowers viscosity. With increased influence from the elastic nature of the polymer, more coating defects can occur including wrinkling, curling or voiding. If the adhesive has met the level of voiding, then the molecular structure of the adhesive has failed and the adhesive cannot be coated thinner. In other words, you have developed swiss cheese and there is no going back.

        EQUIPMENT DESIGN

        So how do you develop the best equipment for such a complex application? Computer modeling. To develop an understanding of this three dimensional equation of stress relaxation and viscosity response, finite element analysis can provide a window into handling hot melt adhesives properly. Without computer modeling, the manifold design will not take into account the complex nature of the adhesive rheology and internal flow characteristics developed in manifold geometries with a slot die.

        Unlike ambient liquids that have self-leveling capability, hot melt adhesives need to be shaped and molded into the final application of a precision coated substrate. However, this shaping and molding needs to be gentle enough not to develop additional and unnecessary stresses.

        The biggest variable controlling how the hot melt adhesive is shaped and molded is the lip opening. To reduce stresses on the adhesive, the lip opening needs to be wide enough to not place undue forces on the polymer melt, but narrow enough to distribute the flow evenly across the width of coating. The lip opening is the most powerful variable in coating because it is the only adjustment that is volumetric in nature. As the lip opening is changed the resulting volumetric flow has a cubic effect on forces acting on the fluid. All other equipment variables are linear.

        That doesn’t mean that the other equipment variables should be ignored. External to the slot die, the gap between the slot die and the substrate needs to be maintained flat and even to maintain a flat and even coating appearance. Because heat causes the metal to move, die bending adjusters may be required to flatten out the front face of the slot die to match the flatness of the substrate or backing roll. As hot melt adhesives are coated and influence the other equipment, by heating the backing roll, the slot die flatness may need to be further adjusted to match the contours of the steady state position of the equipment. So, unlike ambient temperature liquid coating, hot melt coating may have more variation at start-up. The faster the equipment can get to steady state, the less waste will be developed.

        OPERATION

        So once the equipment is at steady state, what do you do if coating defects still persist? One common coating defect in hot melt coating is ribbing; where the adhesive is confused as to whether to stick to the substrate or the slot die. In this case, decreasing the gap between the slot die and the substrate may encourage the adhesive to follow the substrate path. If this isn’t enough, the attack angle of the slot die can be adjusted. The attack angle is the rotation of the slot die around the lower corner of the upper lip of the slot die. This rotation will allow the lip faces to have the desired effect of improved meniscus development without the interference of the slot die with other components.

        When coating rubber bands, there are going to be some limitations to the ability to coat the rubber bands fast and thin. The current upper limit of speed that I am aware of is 3280 feet/min (1000 m/min). This speed limitation seems to be more associated with cooling capability, but the speed could be lower for a thinner coating because of the stresses involved in the take-away process. This is a multi-variable problem and as the thickness of the adhesive coating decreases, the top speed will decrease also.

        The coating thickness of the adhesive is strongly connected to the internal strength of the adhesive. An adhesive chemistry can vary widely, and the effect on the ability to coat thin varies with the molecular character of the polymer. If fillers are added to produce a lower cost adhesive, the coating thickness achievable will rise. It is a balance between raw material costs and processability. For most adhesives, it is safe to assume that 1 mil (25.4 microns) or thicker can be coated. To coat thinner, tests should be run on the adhesive coating capability on a lab or pilot scale line to show proof of concept. I have seen some lower elasticity hot melts coat as thin as 0.5 mils (12.7 microns) successfully.

        Hot melt adhesives coat thicker also, but there are three main levels that coating can be grouped-

        • 3 mils (76.2 microns). In this region, a standard flexible lip slot die lip set should be utilized.
        • 1-3 mils (25.4-76.2 microns). In this region, a rotary rod lip set should be utilized.
        • < 1 mil (25.4 microns). In this region, a rotary rod lip set should be used, but is not guaranteed to have success.
        • In the thicker regime, coating with a standard lip set would allow for a proximity coating technique. In proximity coating, the slot die is positioned the coating thickness away from the substrate with a precision backing roll supporting the substrate. The tall lip faces of 0.15-0.30 inch (3.81-7.62 mm) allow the formation of a meniscus and the sharp lip edges allow for release of the adhesive from the slot die.

          When the coating required drops below 3 mils (76.2 microns), a rotary rod lip design should be utilized to have streak free coating. Without the rotary rod lip design, the lip opening and slot die to substrate gap starts to narrow to the point that adhesive gels or char can develop streaks that are persistent. The way a rotary rod lip set works, the slot die lip face is actually pushed into the backing roll to develop a deflection in the roll. This deflection creates longer path for the substrate to follow, resulting in a slip phenomenon where the adhesive gel or char that would normally get stuck in the narrow gaps clears the path. The backing roll needs to be made of rubber to allow for this deflection. As a general rule of thumb, the thinner you coat, the harder the durometer the rubber should be. It is common to see a 70 Shore A durometer roll for 3 mils (76.2 microns) of coating and a 90 Shore A durometer roll for 1 mil (25.4 microns) of coating.

          As presented in the explanation of the rotary rod lip design, the slot die itself is not the only equipment contributing to the ability to coat precisely. The backing roll, fluid delivery system and slot die positioner all provide some functionality to the success of adhesives coating. In addition, the web handling, tension control and stability of the roll-to-roll coating line can reduce variability or contribute to coating defects. For all equipment involved it is critical to maintain temperature evenly. Variation in temperature translates into variation in rheological characteristics of the adhesive. As the rheology varies, flow varies and the equipment needs to be adjusted to compensate. When at all possible, get to steady state and stay there as long as possible.

          CONCLUSION

          When it comes to fluid coating, there are three options to consider. If the application lends itself to hot melt adhesive coating, keep in mind that you are working in the one area that is the cross section of extrusion and liquid coating. This complex area of operation has a lot of potential, but you need to do your homework to be successful. Understand the limits of the adhesive. Understand the limits of the equipment. Develop the best adhesive for the application and then model the equipment to optimize performance. Hot melt adhesive coating is growing in popularity, so the more you can develop a knowledge base the farther ahead your company will be.

          17 min
        • ROI of Fluid Coating Technology

          /wp-content/uploads/ROI-for-Fluid-Coating-Technology.mp3
          Download Audio File

          When companies are going through the process of justifying a capital expenditure, people need to understand the full cost of ownership (COO). This is fundamentally a return on investment (ROI) question with a life cycle characteristic. Purchase cost combined with operation, utilization and performance can determine the COO for fluid coating equipment. As an example, the calculation of the return on investment (ROI) of a slot die can be developed with some input from the company regarding the details of the products and process in question.

          In order to calculate some of the process variables in coating, it would be helpful to utilize an online calculator located here- https://www.slotdies.com/calculator/. This calculator helps determine the key coating variables for slot die coating utilizing proximity, vacuum assist, or curtain coating. In addition there is a handy roll product calculator that can provide final values for length, weight and area.

          An example of an ROI calculation is presented below for your consideration-

          The ROI calculation is a function of the gain from investment and the cost of investment:

          ROI = (Gain – Cost)/(Cost)

          In this example, the gain from the slot die coating process over the Meyer rod coating process can be obtained from a variety of variables:

          • Line Speed: Slot die coating can operate at increased line speeds. The question of the upper line speed is a function of fluid viscosity that can be determined from trials. The fluid rheology can also be altered to improve process performance. The current maximum line speed for the Meyer rod coating station is 190 m/min. Slot die coating can operate up to 300 m/min.
          • Fluid Waste: Slot die coating operates as a closed system. This necessitates that the fluid being pumped to the coating head is placed on the web. While there are start-up losses, these are relatively the same with slot die or Meyer rod coating techniques. The savings comes from the volume of material in the pan of a Meyer rod system versus the fluid lost in the tubing and manifold section of the slot die.
          • Uniformity: Slot die coating allows for +/- 5% crossweb caliper control in this scenario. Meyer rod coating within the current process allows for +/- 10%.
          • Automation: Looking down the road, the ability to control coating weight via an automated control loop, allows the slot die to be operated within a tight caliper control for a variety of fluids.
          • Question:
            • What are the current limitations in the process? If speed is limited due to the curing system instead of the coating system, then the slot die cannot provide speed improvement capability. If the throughput is limited by the coating technique and fluid rheology capability, then the slot die equipment can provide an improved function.
            • Is uniformity important? If the specification of the product requires +/- 5% versus 10% variation, then slot die equipment would provide an advantage.
            • How much scrap is inherent? If the scrap currently is associated with the coating head, then the slot die can provide a financial improvement on the process.
            • Is it possible to reformulate the fluid? The slot die system provides for an ease of reformulation not recognized in other roll coating techniques. As fluids are varied, the slot die can adjust through mechanical means to work with the fluid within the current parameters of the process. Increasing % solids now becomes an option.
            • Outside of the process cost considerations, there are some operational considerations that need to be answered:

              1. How often does the line run? The start-up and shut-down costs can vary between slot die coating operations and Meyer rod coating operations.
              2. How many operators does it take to run the coating line? Slot die coating and Meyer rod coating may fundamentally require more or less involvement from the operators, depending on familiarity with the system.
              3. What are the material costs? Can reformulation or substrate changes improve ROI?
              4. In the end, the variables listed above can be entered into the ROI formula to develop a bottom line savings number in terms of ROI Months, Adhesive Savings, and Future Savings/Year. The other basic variables required in the ROI formula are: Production Hours/Day, Production Days/Week, Width of Web, Web Speed, Coat Weight, and Adhesive Cost.

                An example is provided below with data provided from a specific coating company that Coating Tech Slot Dies has developed an ROI for in the past and some assumptions:

                Cost of Investment:

                Slot Die (1910 mm) x $60/mm = $114,600 [all prices budgetary]

                Slot Die Positioner = $106,575 [all prices budgetary]

                Precision Backing Roll = $50,375 [all prices budgetary]

                Total = $271,550 [all prices budgetary]

                Gain of Investment:

                Line Speed (Sslot die) = 300 m/min*

                Line Speed (SMeyer rod) = 190 m/min

                Scrap Volume (Vslot die) = 2 L/prod*

                Scrap Volume (VMeyer rod) = 5 L/prod

                Product Scrap (Uslot die) = 500 m/prod*

                Product Scrap (UMeyer rod) = 1000 m/prod

                * = estimated variables

                Use the Coating Tech Slot Dies Technical Calculator to run these calculations. Click here for the link.

                The above ROI calculation can be provided if required for further development of costs. This ROI calculation provides the greater margin driven by higher production capacity. In addition, there are savings associated with improved cycle time benefits (reduced energy cost and labor cost associated with more production time versus reduced scrap) and improved quality benefits (fewer defects, fewer customer returns, and reduced time handling customer complaints). The Cost of Investment takes into account the hardware involved, but this is not the full cost of implementation. The true cost of investment includes training costs, downtime for equipment installation, and ongoing support.

                In this example, an investment in slot die technology would provide a positive ROI if the improvements are deemed valuable enough for the investment. The investment decision is not easy, but the equipment improvement can provide a solid return.

                So, after you know what the price is of a piece of equipment, what is the cost of ownership? Prices can be readily obtained from vendors in the industry, but understanding whether the equipment will truly match the need takes a deeper discussion. Buying equipment for a converting process is not a trivial matter. Invest in questioning the vendor before investing in the product. The 3P approach to vendor selection has guided many of these discussions in the past and can help lead you down the path of a successful purchase for your converting application. Combining 3P with ROI, leads you to a strong understanding of capital investment.

                If you are interested in discussing this concept further, contact Mark D. Miller, Founder and CEO of Coating Tech Slot Dies, LLC (www.slotdies.com) at [email protected] or (715) 456-9545.

                8 min
              5. Balancing Slot Die Design
                /wp-content/uploads/balancing_slot_die_design_for_improved_flow_control_and_reduced_coating_defects.mp3
                Download Audio File

                Wouldn’t life be great if complex things could be reduced to simple functions? In the world of coating, if you look deep enough, you can find some of these useful nuggets.

                In self-metered coating, the liquid flow can be studied as a collection of bulk flow and flow along surfaces. At the surface, there are forces fighting over whether the fluid should move forward, sit still, or swirl in place. But why is this important?

                Let’s look at the final coated product and work our way back to the equation. Let’s assume you are coating an emulsion adhesive and there is a pesky streak on the coated web. Where did it come from? There are many potential factors, including dirt, gels, bubbles, a nick in the flow surface, or one of many equipment issues.

                To decide where to start, you would want to eliminate the obvious first and work your way to the more complicated. Stop the coating line, check the manifold for particles stuck in the gaps and loading of filters in the fluid flow lines. Inspect the flow surfaces and clean the system. Now that these are eliminated, what can we look at if the streak persists?

                One area to consider is the geometry of flow within the slot die. The flow channels of a slot die can be simplified and studied like an air duct. When the air duct is a rectangular shape, like the exit of the slot die onto a substrate, the following equation applies:

                τw = wall sheer stress

                μ = viscosity

                V = volumetric flow rate

                b = slot gap

                When wall sheer stress is greater than the shear stress through the system, then particles will choose to move forward instead of sit on the flow surface. The bulk shear stress for most fluids is approximately 1 N/m2. This means that agglomeration of particles will not occur and streaks will not form if the wall shear stress is greater than this level.

                This equation typically requires computer simulation to verify, but the power of the equation is simple – if the volumetric flow rate is too low, viscosity too low, or gap too large, the wall sheer stress may not be enough to clean the system.

                If you have consistent streaks in the coating, consider increasing the flow rate, viscosity, or narrowing the gap. If the equation is balanced, the contamination will be less likely to occur, and splitting and cleaning the die will not be as critical a step between product changes.

                But remember: these factors need to be balanced with the other needs of the flow control. Slot die operation is a balance between variables and control factors that can develop an excellent thin film or one full of coating defects. Pressure drop, fluid velocity, volumetric flow rate, and shear effects need to be in the proper coating window for optimized operation.

                4 min
              6. Dispersions in Liquid Coating
                /wp-content/uploads/dispersions_in_liquid_coating.mp3
                Download Audio File

                Liquids can be described as mayonnaise or beer. The Newtonian fluids are beer – they are self-leveling and if you turn a glass of beer upside down, the beer spills out. The non-Newtonian fluids are mayonnaise – without shear they will not move. Turn the mayonnaise jar upside down and it goes no where. But what happens when you have a wheat beer, or a garlic aioli? The dispersed particles can cause coating defects you weren’t expecting.

                Depending on the industry, particles in fluid coating can be common or unusual, but it is good to consider them if you coat fluids for a living, because the particles can add functionality and premium products. In the battery industry, cathodes and anodes are highly filled slurries, where particles are common place. This is also true with microspheres in adhesive coating and nanowires in ITO replacement film. The reality is particles are getting smaller and more important for functionality of active fluid coatings.

                While non-functional particles in coating can create defects and are typically filtered out, functional particles need to be included in the coated product and special care needs to be taken to make sure the equipment is designed properly and the process is set up for success. There are a couple key items to consider when dealing with dispersions-

                Residence time. Fluids that have particles dispersed throughout the liquid matrix have a residence time before they fall out of suspension. Have the fluid sit for too long and you will be coating a liquid without the functional component while it sits in the bottom of a pan or a slot die manifold that is too large for the application conditions.

                Agglomeration. Particles can stick to each other if the initial mixing of the fluid with particles is done improperly, but it can also occur because of the coating process. Depending on the size and type of particles and the fluid and the loading of the particles, initial agglomeration can be avoided with proper mixing. Proper mixing may mean aggressive mills or simple agitation. Once the particles have been dispersed, they need to stay dispersed, so either movement, agitation or chemical separators should be considered. For shear sensitive particles, excessive agitation or the shear of too narrow a slot gap can cause a agglomeration.

                In each of these instances, the simulation of the flow of the dispersion through the system can provide insight into the excessive residence time, the shear zones or other areas of concern for agglomeration or particles falling out of suspension. So whether you are dealing with beer or mayonnaise, if the fluid is loaded with dispersed particles, dig deeper to understand the material reaction to the process and the design behind the equipment to ensure precise coating capability.

                3 min
              7. The Critical Variable – Slot Die Lip Gap
                /wp-content/uploads/the_critical_variable-slot_die_lip_gap.mp3
                Download Audio File

                It’s important to pay attention to critical variables in coating. When it comes to slot die setup and operation, the variables can be separated into linear variables and cubic variables. As you can imagine, linear variables affect the coating performance some, but the cubic variables have a stronger effect. So what affects coating on this larger scale?

                To answer that question, we have to understand how the fluid is being controlled as it passes through the slot die to exit onto the substrate. While the manifold of the slot die distributes the fluid uniformly within the slot die, the lip land and slot die lip gap controls the final fluid flow as it exits the slot die. The key to uniform flow is distribution and stable pressure, velocity, and volumetric flow at exit. The governing equation for flow is shown here:

                Where the variables are defined:

                • ΔP = pressure drop through the slot die
                • b = slot die lip gap
                • μ = viscosity
                • L = lip land length
                • The slot die lip gap, or feed slot opening, is the only variable to the power of 3. When this variable shifts, the result is your strongest lever of control. The slot die is typically designed as two pieces of metal that are either separated by a body shim or adjusted by lip adjusting bolts working against a hinged lip design.

                  When the slot die lip gap is reduced, the back pressure increases, the velocity increases, and the cross web caliper control typically improves. You have to be careful with shear sensitive fluids however, and manage the flow control with the rheological properties.

                  So what does this mean to the slot die operator? It means that a small change goes a long way. If you have a fixed lip slot die that utilizes a body shim to control the fluid flow, then the difference between different body shim thicknesses are compounded by the flow control equation. Many coating trials start with one shim dimension, that if unsuccessful, the engineer wants to change by an order of magnitude. This simple equation shows that the slot die lip gap change (and the subsequent shim thickness) should be shifted slightly to see the effect.

                  Similarly, if you are operating a flexible lip slot die, it is important to start with the lip opening at a well tuned opening via feeler gauges and remember that a small adjustment can create a large effect. Typically, an operator is adjusting a flexible lip slot die while watching the results on a gauging system. You need to be careful here, because the response time for the cross-web gauge and the fluid flow control will not be instantaneous. I would caution the slot die operator to make a minor change and then wait for the response to show before chasing the high or low spot in coating.

                  In the end, if you understand the math behind the fluid flow, you understand the controlling variables that represent the parts of the equipment that control the process. Every little piece of information helps coating and, in this case, some small variable changes can have large effects.

                  4 min
                • Smart Glass Coating Technology
                  /wp-content/uploads/smart_glass_coating_technology.mp3
                  Download Audio Filehttps://www.slotdies.com/wp-content/uploads/Smart-Glass-Video.mp4

                  All modern products and equipment are getting smarter. There are internal computers tracking automotive mechanics as we drive, there are feedback loops in what we search online and there is the ubiquitous “internet of things.” Construction materials are no exception. Glass for residential and commercial buildings now have options beyond the standard glazed low emission glass of yesteryear. Now you can simply flick a switch and turn a clear glass panel from transparent to opaque. In some cases, the glass can also be tune-able for the proper amount of translucency. You can imagine how this technology can be connected with motion, light or heat sensors to have the glass respond to the environment.

                  How is this possible? Of course the invention relies on precision coating techniques. In addition to requiring glass handling and calculated drying and curing technology, precision coating techniques need to be considered to make a glass panel a “smart” glass panel.

                  Smart or switchable glass utilizes a coating of suspended particles or energy altered chemistry to change the state of the glass through human control.

                  The coating techniques and process understanding for glass panel coating is not trivial. In addition to coating a discrete substrate versus a continuous one, the coating thicknesses required are thin. The thinner you coat, the more precision matters.

                  Intermittent coating. When coating a glass panel, the first push of fluid out of a coating head needs to be balanced in pressure in order to create a flat even coating bead for application. This means that the fluid delivery system is balanced, macro and micro bubbles need to be controlled, and the velocity of the fluid needs to be delivered evenly across the width of the coating head. This can be done with a continuous loop of fluid that is diverted at the point of application, or with a controlled single shot pump that is balanced in feed rate and pressure.

                  Proximity coating. If dry edges or patterns are required on the glass panel, the ability to position a coating head in close proximity to the panel must be done. An alternative is to mask the glass prior to coating. The difficulty with proximity coating glass is the thin coating requires close proximity to an uneven surface. Glass is not very flat and typically cannot be held with too much force or it will break. So if proximity coating is required for the application, precision of manufactured surfaces (both the coating head and the substrate holder) are required.

                  Curtain coating. When various width glass is to be run or a dry edge is not required, curtain coating is an excellent option. The best approximation of the line speed required for the fluid is provided by the Weber number calculation-

                  ρ = density

                  Q = volumetric flow rate

                  V = impingement velocity

                  σ = surface tension

                  If the Weber number is greater than 2, theoretically the fluid should form a curtain.

                  Cleanliness. When coating glass, the need to keep the panel clean with multiple handling steps becomes complicated. Keeping a coating area clean is critical to precision coating. The more there is human interaction, the more the area is contaminated.

                  Variable substrate thickness. No matter how consistent the panel supplier, in order to coat thin fluids onto glass, you need to be concerned about variable thicknesses. The panel coater needs to account for the substrate variation and set the coating head appropriately.

                  These are a few of the considerations one should look at when considering thin fluid coatings onto glass. If the active fluid has suspended particles, then proper mixing, filtration and recirculation should also be considered. While smart glass is amazing, the complexity of the coating technique is also amazing.

                  Not only utilized in commercial building structures, the use of smart glass can be utilized in automotive, aerospace and marine applications. As the material development, customer requirements and product uses become more precise, controlled and “smart,” you need to expand your understanding of precision coating to keep up.

                  5 min